Introduction:Suitable for welding Ni9%(UNS K81340) alloy,dissimilar steels as well as welding problem metals.
Standard &Typical Chemical Composition of Deposited Metal (%)
Element
|
C
|
Mn
|
Si
|
Fe
|
S
|
P
|
Cu
|
Ni
|
Nb+Ta
|
Al
|
Mo
|
Cr
|
Other element
|
Specification
|
≤0.10
|
2.00-4.00
|
≤1.00
|
≤10.0
|
≤0.020
|
≤0.030
|
≤0.50
|
≥55.0
|
0.5-2.0
|
-
|
5.0-9.0
|
12.0-17.0
|
W1.0-2.0
|
Actual Result
|
0.017
|
3.20
|
0.18
|
5.5
|
0.010
|
0.005
|
0.10
|
60.00
|
0.86
|
-
|
7.00
|
13.80
|
1.30
|
Standard & Typical Properties of Deposited Metal
Test Item
|
Tensile Strength Rm (MPa)
|
Elongation A(%)
|
Akv Value (J)
|
Specification
|
≥620
|
≥35
|
-196℃ ≥30 |
Actual Result
|
680
|
40
|
130
|
Size and Current (DC +)
Dia.(mm)
|
2.5
|
3.2
|
4.0
|
Length(mm)
|
250
|
300
|
350
|
Current(A)
|
50-70
|
80-100
|
110-150
|