Introduction:Suitable for welding ship hulls, pressure vessels,bridges as well as structural fabrications.
Standard & Typical Chemical Composition of Deposited Metal (%)
Chemical Composition
|
C
|
Mn
|
Si
|
S
|
P
|
Cr
|
Ni
|
Mo
|
V
|
Specification
|
≤0.20
|
≤1.20
|
≤1.00
|
≤0.035
|
≤0.040
|
≤0.20
|
≤0.30
|
≤0.30
|
≤0.08
|
Actual result
|
0.094
|
0.51
|
0.27
|
0.018
|
0.028
|
0.054
|
0.052
|
0.004
|
0.012
|
Standard & Typical Mechanical Properties of Deposited Metal (AW)
Test Item
|
Yield Point ReL (MPa)
|
Tensile Strength Rm(MPa)
|
Elongation A4(%)
|
Akv Value (J)
|
Specitication
|
ReH≥306
|
400-560
|
≥22
|
0℃ ≥47
|
Actual Result
|
385
|
480
|
29
|
59
|
Size and Current(AC or DC)
Dia.(mm)
|
2.5
|
3.2
|
4.0
|
5.0
|
Length(mm)
|
300
|
350
|
400
|
400
|
Current(A)
|
40-70
|
100-130
|
150-200
|
190-240
|